What problems might arise during the production of silicone heating wire cables?
Release Date:
2021-11-04
Author:
Abstract:
Silicone heating wires, owing to their high heat resistance and excellent cold resistance—allowing a long-term operating temperature range of −90 to 250°C—as well as superior electrical insulation and aging resistance, have experienced rapid growth in the cable industry.
Issues encountered in the production of silicone heating wire cables:
1. Rubber after sulfur blending is prone to scorching during extrusion and contains a large amount of impurities, which can lead to dielectric breakdown.
2. During the sheath extrusion process, shell loosening and bubbling may occur.
Solution:
1. Technical Requirements for Mixing and Remanufacturing
Although the processing equipment for silicone heating cables is essentially the same as that used for organic rubber, do not use the same open‑mill to process both organic rubber and silicone heating cables. Dedicated cleanroom facilities are required to maintain a pristine environment, as contamination can degrade the mechanical and electrical properties of the silicone heating cable. If dedicated processing equipment and facilities are unavailable, ensure that any contaminating materials are kept entirely separate from the silicone heating cable and its additives, since most impurities originate during the rubber‑mixing stage.
Due to the inherent properties of silicone heating wires, the plasticity of the reclaimed rubber changes after reprocessing, and it can easily adhere to the mixing drum at a relatively rapid rate. The drum of an open‑type mixer should be filled with cooling water to prevent the rubber from scorching.
To obtain high-quality products, the following basic steps should be followed during the mixing process of silicone heating wires:
(1) Accurately weigh each component to be used (e.g., flame retardant, vulcanizing agent, color masterbatch, etc.).
(2) Place the silicone heating wire or reinforced rubber on an open‑air mill, adjust the nip gap so that the silicone heating wire is tightly wound around the rolls at high speed, and carry out thorough refining. Pure silicone heating wire may be compounded with fillers either before or after re‑refining. However, since reinforced silicone heating wire contains silica, it must undergo thorough refining.
(3) If necessary, flame retardants and color masterbatches should be added to the compound. During mixing, some fillers may fall into the receiving pan via the mixer drum. Before adding the next batch of filler, these materials should be collected and reintroduced into the rubber. A rubber scraper is typically used to remove the filler from the receiving pan; brushes should not be employed, as bristles may shed and contaminate the rubber. It is particularly important to note that all fillers should not be added to the compound in a single charge; instead, they should be introduced in 2–3 separate batches. When adding each batch, the compound must be thoroughly turned over.
(4) Add the vulcanizing agent to the compound. Do not add the vulcanizing agent when the rubber is too hot (not exceeding 40°C), as this may cause premature partial vulcanization, resulting in losses of both rubber and vulcanizing agent. Introduce sufficient cooling water into the roll to prevent the rubber from overheating. To ensure uniform dispersion of the curing agent, the entire roll of rubber should be diluted several times.
Recommended Reading
Spring Heating Wire: A Warm and Harmonious Companion for the Family